MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® Terra HS 16 natural Nylon 610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: VESTAMID Terra HS16 natural color is a medium-viscosity PA 610 basic polymer for monofilaments and bristles with high recovery for paint brushes and tooth brushes. The carbonamide groups (-CO-NH-) of the polyamides form hydrogen bridge bonds between the chains of the macromolecules, thereby substantially promoting crystallinity and increasing their strength, melting point, resistance to chemicals and water absorption. This is characteristic of all semicrystalline polyamides . Because of its semi-crystalline morphology VESTAMID Terra HS16 natural color provides a high impact strength, excellent chemical resistance (e.g. against greases, oils, alkalis and saline solutions), a low coefficient of friction and high abrasion resistance. Properties of VESTAMID Terra HS16 natural color vary little with changing humidity due to their low moisture absorption. VESTAMID Terra HS16 natural color is supplied as cylindrical granules, ready for processing, in moisture-proof bags. VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is extracted from castor oil, VESTAMID® Terra HS is based on natural, renewable resources up to 62%.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Water Absorption at Saturation 3.3 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 61.0 MPaISO 527-1, ISO 527-2
Elongation at Break >= 50 %ISO 527-1, ISO 527-2
Elongation at Yield 5.0 %ISO 527-1, ISO 527-2
Tensile Modulus 2100 MPaISO 527-1, ISO 527-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1 eU
 NB
@Temperature -30.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 6.00 kJ/m²
@Temperature -30.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C2nd heating, DSC; ISO 11357
Vicat Softening Point 196 °C
@Load 5.10 kg
Method B; ISO 306
 220 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
Global Warming Potential (kgCO2 equivalent/kg material)4.1Evonik, PE International, preliminary data
Renewable Carbon (%)62ASTM 6866

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 610
Evonik VESTAMID® NRG 1001 PA 12
Evonik Vestamid® Terra HS 22 natural color Nylon 610
Overview of materials for Nylon 612, Unreinforced
Overview of materials for Polypropylene Copolymer

PEVONIK986 / 192749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.