MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Alliance BCS-4 Samarium Cobalt Compression Bonded Magnet
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy

Material Notes: Samarium Cobalt Compression Bonded Magnets are one of the newest types of magnetic materials and are made by compressing an epoxy coated SmCo magnet powder into a final shape and then heat treating it. The result is a high density material which produces a higher magnetic output than by injection molding. Although compression molding provides greater flexibility in geometry shape and size, they do not provide the range of complex geometries which can be achieved by injection molding.

Information provided by Alliance LLC.

Key Words: Permanent SmCo Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.40 - 7.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80 - 125
Modulus of Elasticity 29.0 GPa
Compressive Strength 30.0 - 32.0 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0400 ohm-cm
Magnetic Coercive Force, Hc 2500 - 3500 Oe
 8000 - 13000 OeIntrinsic
Magnetic Remanence, Br 3800 - 4200 Gauss
Magnetic Maximum Energy Product, BH 3.5 - 4.5 MGOe
Curie Temperature 700 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 150 °CContinuous
 
Descriptive Properties
Reversible Temperature Coefficients-0.035Bd. %/°C
 -0.29Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NALLIAN9904 / 268440

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.