MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arla MULTICLEAR® Box 2 Wall HG PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MULTICLEAR® Box 2 Wall HG is a range of extruded multiwall polycarbonate sheet specifically designed to offer increased transparency combined with solid rigidity. Resulting in cost saving by using less glazing bars for installations hence increased light transmittance. MULTICLEAR® BOX 2 Wall HG is a transparent or translucent sheet with one side UV protection (also available with two side UV protection). Standard available in clear, opal and bronze. Available in thicknesses 16 mm only. Knife cutting operation is used both online and offline to avoid saw dust. MULTICLEAR® BOX 2 Wall HG has a 10 year limited warranty against discoloration, loss of impact strength and light transmission due to weathering.

Benefits: Less structural glazing bars hence increased light transmission; Large rib distance offering greater transparency; Good wind and snow loading capacity; Aesthetic glazing

Application: Building industry – roofing, cladding, sidewalls, conservatories, domes, skylights, sheds, car ports, swimming pool covers, suspended ceilings, glasshouses, railway/metro station, stadia roofing and partitions. Lighting/packaging lamp optics and protective covers for fragile items. Advertising – illuminated signs and advertising panels. Agriculture greenhouses, lorry/tractor ports and farm/barn buildings.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.80 W/m-K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA920 / 301098

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.