MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide
Categories: Metal

Material Notes: Construction: Expanded Metal in Elastomer

Available Forms: Sheets, Die-Cut Gaskets

Standard Metals Available in EMI Portion: Monel Aluminum

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  >= 35 dB
@Frequency 14000 Hz
>= 35 dB
@Frequency 14000 Hz
 >= 85 dB
@Frequency 1e+9 Hz
>= 85 dB
@Frequency 1e+9 Hz
 >= 102 dB
@Frequency 1.80e+7 Hz
>= 102 dB
@Frequency 1.80e+7 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FSilicone Version
Minimum Service Temperature, Air -62.0 °C-79.6 °FSilicone Version
 
Descriptive Properties
Maximum Joint Unevenness, % of Gasket Height0.1Class B- Open-Close in Same Position
 0.1Class C- Completely Interchangeable
 0.15Class A- Permanently Closed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nye Lubricants 759QR-12 (NG) Synthetic Oil
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Chosun Refractories A50 Special High-Density Gunning Castable
AISI 1018 Steel, hot rolled, quenched, and tempered

PCHOME295 / 131005

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.