MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro DESMODUR® MTR31130 + BAYTEC® RT9234, 70 D Polyurethane, MDI- PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccBAYTEC® RT9234, B
 1.02 g/cc1.02 g/ccBAYTEC® RT9234, A
 1.10 g/cc1.10 g/ccDESMODUR® MTR31130
 1.16 g/cc1.16 g/cc
Viscosity 75 cP75 cPBAYTEC® RT9234, B
 750 cP750 cPBAYTEC® RT9234, A
 800 cP800 cPDESMODUR® MTR31130
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070DIN 53505
 64
@Temperature 80.0 °C
64
@Temperature 176 °F
DIN 53505
 74
@Temperature -5.00 °C
74
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 44.0 MPa6380 psiDIN 53504
Tensile Stress at Strain 22.6 MPa
@Strain 10 %
3280 psi
@Strain 10 %
DIN 53504
Elongation at Break 215 %215 %DIN 53504
100% Modulus 28.9 MPa
@Strain 100 %
4190 psi
@Strain 100 %
DIN 53504
200% Modulus 51.2 MPa
@Strain 200 %
7430 psi
@Strain 200 %
DIN 53504
Resilience 5050[%]; DIN 53512
Tear Strength 76.0 kN/m434 pliwith nick; ISO 34-1
 153 kN/m873 pliwithout nick; ISO 34-1
Abrasion 5555[mm3]; ISO 4649
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FDESMODUR® MTR31130
 45.0 °C113 °FBAYTEC® RT9234, A
 45.0 °C113 °FBAYTEC® RT9234, B
Pot Life 10.0 min10.0 min
 
Descriptive Properties
AppearanceliquidDESMODUR® MTR31130
 solidBAYTEC® RT9234, A
 solidBAYTEC® RT9234, B
Content100Parts by weight of prepolymer
 12.9-13.3%NCO, DESMODUR® MTR31130
 43.5Parts by weight of BAYTEC®RT923x

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0554 / 202337

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.