MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cambrios Technologies ClearOhm™ Coating Material
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: ClearOhm coating material is a engineered nanomaterial aqueous solution that produces a transparent/conductive film by wet processing. Applications of ClearOhm coating material include transparent electrodes for touch screens, liquid crystal displays, e-paper, OLED devices, and thin film photovoltaics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cc
Solids Content 0.050 - 3.0 %
Filler Content 0.10 - 5.0 %Silver (Ag)
Particle Size 0.010 µm
Viscosity 1.0 - 100 cP
Surface Tension 39 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 10 - 500 ohm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88 - 92 %
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 1800 sec
 
Descriptive Properties
AdhesionPasses
Binder SystemPolymer
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesOptical grade
Solvent SystemAqueous and Solvents

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFLEXCM47 / 179449

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.