MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Lupranate® 5070 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® 5070 Isocyanate is a low functional prepolymer based on pure MDI. Lupranate 5070 isocyanate is favored in solid elastomers and microcellular foams where the formulator desires good abrasion resistance over a wide range of temperatures. The relatively low viscosity at room temperature can simplify the handling and preparation of one-shot cast elastomer such as wheels, rollers, and mats.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Viscosity 3360 cP3360 cP
Vapor Pressure 1.33e-8 bar
@Temperature 25.0 °C
0.00000998 torr
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
>= 374 °F
@Pressure 0.0967 psi
Flash Point 200 °C392 °F
 
Descriptive Properties
ColorYellow
CompositionNCO content0.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Lupranate® 5090 Isocyanate
BASF Lupranate® 5080 Isocyanate
BASF Lupranate® 5060 Isocyanate
BASF Lupranate® 5050 Isocyanate
BASF Lupranate® 5040 Isocyanate

PBASG0675 / 132308

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.