MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.29 - 1.96 g/ccAverage value: 1.48 g/cc Grade Count:24
Filler Content 10.0 - 50.0 %Average value: 24.5 % Grade Count:10
Water Absorption 0.0200 - 0.200 %Average value: 0.0575 % Grade Count:8
Water Absorption at Saturation 0.0400 - 0.100 %Average value: 0.0850 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00860 cm/cmAverage value: 0.00276 cm/cm Grade Count:18
Linear Mold Shrinkage, Transverse 0.00330 - 0.00800 cm/cmAverage value: 0.00653 cm/cm Grade Count:8
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 67.6 - 680 MPaAverage value: 207 MPa Grade Count:22
Elongation at Break 0.500 - 100 %Average value: 5.96 % Grade Count:20
Modulus of Elasticity 9.50 - 55.0 GPaAverage value: 22.3 GPa Grade Count:17
Flexural Yield Strength 55.0 - 780 MPaAverage value: 278 MPa Grade Count:19
Flexural Modulus 0.552 - 57.0 GPaAverage value: 18.3 GPa Grade Count:20
Flexural Strain at Break 1.30 - 2.90 %Average value: 2.05 % Grade Count:4
Compressive Yield Strength 650 MPaAverage value: 650 MPa Grade Count:3
Compressive Modulus 51.0 - 51.0 GPaAverage value: 51.0 GPa Grade Count:3
Shear Strength 131 MPaAverage value: 131 MPa Grade Count:3
Izod Impact, Notched 0.374 - 0.481 J/cmAverage value: 0.423 J/cm Grade Count:6
Izod Impact, Unnotched 1.60 - 3.74 J/cmAverage value: 2.67 J/cm Grade Count:5
Izod Impact, Notched (ISO) 6.00 - 6.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 6.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 31.0 - 31.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 31.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.70 - 2.20 J/cm²Average value: 1.94 J/cm² Grade Count:8
Charpy Impact, Notched 0.350 - 0.600 J/cm²Average value: 0.496 J/cm² Grade Count:5
Coefficient of Friction 0.0400 - 0.270Average value: 0.144 Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00820 - 10000 ohm-cmAverage value: 2790 ohm-cm Grade Count:13
Surface Resistance 10.0 - 1.00e+6 ohmAverage value: 251000 ohm Grade Count:8
Insulation Resistance 1000 - 1.00e+6 ohmAverage value: 667000 ohm Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 - 32.0 µm/m-°CAverage value: 14.2 µm/m-°C Grade Count:10
 30.0 - 30.0 µm/m-°C
@Temperature 150 - 250 °C
Average value: 30.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 5.00 - 47.0 µm/m-°CAverage value: 25.3 µm/m-°C Grade Count:4
 60.0 - 60.0 µm/m-°C
@Temperature 150 - 250 °C
Average value: 60.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.700 - 38.0 W/m-KAverage value: 9.98 W/m-K Grade Count:3
Melting Point 278 - 285 °CAverage value: 281 °C Grade Count:13
Maximum Service Temperature, Air 185 - 260 °CAverage value: 237 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 260 - 285 °CAverage value: 273 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 232 - 280 °CAverage value: 261 °C Grade Count:14
Vicat Softening Point 104 - 255 °CAverage value: 196 °C Grade Count:3
Glass Transition Temp, Tg 60.0 - 90.0 °CAverage value: 85.7 °C Grade Count:7
Flammability, UL94 HB - V-0Grade Count:14
 
Processing PropertiesOriginal ValueComments
Processing Temperature 285 - 350 °CAverage value: 312 °C Grade Count:5
Nozzle Temperature 320 - 340 °CAverage value: 330 °C Grade Count:3
Melt Temperature 285 - 360 °CAverage value: 322 °C Grade Count:11
Mold Temperature 120 - 180 °CAverage value: 149 °C Grade Count:13
Drying Temperature 50.0 - 150 °CAverage value: 123 °C Grade Count:15
Injection Pressure 30.0 - 124 MPaAverage value: 88.8 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler

O4521 / 78344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.