MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cotronics 4420 One-Part Epoxy
Categories: Polymer; Thermoset; Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Moisture Absorption at Equilibrium 0.50 %0.50 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Tensile Strength, Ultimate 48.3 MPa7000 psi
Elongation at Break 1.5 %1.5 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cm
Dielectric Strength 15.7 kV/mm400 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C
@Temperature 20.0 °C
25.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.15 W/m-K8.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C450 °F
Shrinkage 0.30 %0.30 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 121 °C
0.500 hour
@Temperature 250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast Saf-T-Poxy 2410 / 2183 Epoxy
Fibre Glast 2000 / 2020 System 2000 Epoxy
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Elantas Conap FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener
Covestro Desmocap® 11 A Epoxy Coating

PCOTR0460 / 29071

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.