MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® U 241 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Polyester polyurethane dispersion. In the formulation of stoving industrial coatings, stoving automotive primer surfaces and two-pack polyurethane primers and top coats for plastics.

Properties / Applications: Bayhydrol® U 241 is a polyester polyurethane dispersion neutralized with dimethyl ethanol amine which is resistant to hydrolysis. The product can be diluted with water for application and shows no dilution anomalies. Bayhydrol® U 241 can be combined with partially methylated melamine resins to formulate water-dilutable stoving coatings and primers which cure at approx. 120 °C. The ratio of Bayhydrol® U 241 to the amino resin (calculated on the solvent-free resin) is usually 75 : 25 to 70 : 30. Because of the huge amount of commercial available amino resins, compatibility should always be tested.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccDIN EN ISO 2811-2
Volatiles 58 - 60 %1g/1h/125°C; DIN EN ISO 3251
Particle Size >= 50 µm
pH 6.5 - 8.51:3 in demineralized water; DIN ISO 976
Viscosity 500 - 1500 cPD= approx. 40 s-1; DIN EN ISO 3219/A.3
 
Chemical PropertiesOriginal ValueComments
Acid Value 3.8 - 8.5[mg KOH/g]; DIN EN ISO 2114
 
Descriptive Properties
Appearanceopalescent to milky-brownish/cloudy
Content2.5%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0164 / 201947

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.