MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping

Automotive Specifications: Chrysler MS-DB590 CPN4660; Ford WSB-M4D734-A

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inASTM D955
 0.013 cm/cm0.013 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 959515 seconds; ASTM D2240
Hardness, Shore D 424210 seconds; ASTM D2240
Tensile Strength, Yield 7.58 MPa1100 psiType 1, 20 in/min; ASTM D638
 10.3 MPa1490 psi2.0 in/min; ASTM D638
Tensile Stress at Strain  8.41 MPa
@Strain 100 %
1220 psi
@Strain 100 %
2.0 in/min; ASTM D412
 8.55 MPa
@Strain 300 %
1240 psi
@Strain 300 %
2.0 in/min; ASTM D412
Elongation at Break 140 %140 %Type 1, 20 in/min; ASTM D412
 550 %550 %2.0 in/min; ASTM D412
Elongation at Yield 16 %16 %Type 1, 20 in/min; ASTM D638
Flexural Modulus 0.290 GPa42.1 ksiASTM D790
Poissons Ratio  0.337
@Temperature -35.0 °C
0.337
@Temperature -31.0 °F
ASTM D638
 0.363
@Temperature 85.0 °C
0.363
@Temperature 185 °F
ASTM D638
 0.419
@Temperature 23.0 °C
0.419
@Temperature 73.4 °F
ASTM D638
Izod Impact, Notched NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D624
Gardner Impact 33.9 J
@Temperature -30.0 °C
25.0 ft-lb
@Temperature -22.0 °F
ASTM D3029
Tensile Impact Strength 470 kJ/m²224 ft-lb/in²ASTM D1822
Tear Strength 63.8 kN/m364 pliDie C; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 119 µm/m-°C
@Temperature -30.0 - 30.0 °C
66.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature -30.0 - 30.0 °C
65.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 62.8 °C145 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 40.6 °C105 °FUnannealed; ASTM D648
Glass Transition Temp, Tg -55.9 °C-68.6 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive
Taiwan PU Corporation TPU-E95 General Grade, Extrusion Molding Polyester Base TPU
Spartech Formalloy TPR Thermoplastic Rubber Alloy Specialty Sheet
Polymax® Maxelast® C4800 TPE, Transparent

PTEKNP569 / 129642

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.