MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® eXten D247 F Nylon 66 & 610
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Polyamid 66 & 610, impact modified, alkali resistance, mold release, for injection molding. This material is available in natural color and in colors on request

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: TECHNYL® eXten D 247 is used in all sectors of industry, offering high impact strength & excellent productivity. This product is especially suitable for the following purposes: Battery gaskets.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D786
Tensile Strength, Yield 60.0 MPaASTM D638
Elongation at Break 40 %ASTM D638
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 2600 MPaASTM D790
Izod Impact, Notched 210 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 182 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °CASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
ISO 1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, Conditioned
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, Conditioned
Domo TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY
Domo TECHNYL® 2412GHF8 PA66, 40% glass fiber, Conditioned
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY

PRHOD555 / 137786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.