MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 7014 Performance Paper Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmness and strength on a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics, as well as, metals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.900 milAdhesive
 1.90 milFacestock
 2.50 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 0.6875 pliPolypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
 0.875 pliLD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 1.25 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 1.50 pliLD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
 1.6875 pliHD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
 1.6875 pliHD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 1.75 pliHD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 1.8125 pliLD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.00 pliHD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.25 pliLD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.4375 pliPolypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
 2.50 pliHD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
 2.50 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.5625 pliHD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.75 pliLD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
 3.00 pliLD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 3.375 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 50.0 °CApplication
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type320 Acrylic
Liner43# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33425 / 168172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.