Hostacom DYS 707N T 8051 is an unfilled impact modified polypropylene, with good processability and excellent impact/stiffness balance. Product is available as a customized color matched, pellet form. This grade is delivered in 8051 color version. Applications: Interior TrimsInformation provided by LyondellBasell. |