MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco 1583 Polyester, Pellet, Injection Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: PLENCO 01583 is a mineral and glass filled pelletized polyester molding compound, with good arc and track resistance. UL recognized under component file E40654.

Information supplied by Plenco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.86 g/ccASTM D792
Apparent Bulk Density 0.860 g/ccApparent density per ASTM D1895
Water Absorption 0.070 %ASTM D570
Linear Mold Shrinkage 0.0035 cm/cmper ATM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 53ASTM D785
Tensile Strength, Ultimate 60.2 MPaASTM D638
Elongation at Break 1.08 %ASTM D638
Tensile Modulus 10.92 GPaASTM D638
Flexural Yield Strength 96.6 MPaASTM D790
Flexural Modulus 10.09 GPaASTM D790
Compressive Yield Strength 119.4 MPaASTM D695
Izod Impact, Notched 0.330 J/cmASTM D256
Charpy Impact, Notched 0.330 J/cm²ASTM D256
Impact 256J/m Plenco drop ball test
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.911e+14 ohm-cmASTM D257
Dielectric Constant 4.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.0 kV/mmStep by Step; ASTM D149
 14.4 kV/mmShort Time; ASTM D149
Dielectric Breakdown 23000 VHot dielectric breakdown; 1hr/120°C
Dissipation Factor 0.017
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 190 secASTM D495
Comparative Tracking Index 600 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 208 °CHeat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 255 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.47 mm
Shrinkage 0.020 %ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLEL27 / 50595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.