MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® W DP 85085A Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes:
  • injection molding grade
  • no yellowing under the action of UV light
  • improved microbial resistance
  • good low-temperature flexibility
  • Improved hydrolysis resistance
Application
  • automotive interior applications

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Melt Density 0.960 g/cc
@Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 853s; ISO 868
Abrasion 28mm³; ISO 4649
Compression Set 18 %
@Temperature 23.0 °C
ISO 815
 42 %
@Temperature 70.0 °C
ISO 815
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.70 J/g-°CMelt
Thermal Conductivity 0.131 W/m-KMelt
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 220 °C
Mold Temperature 20.0 - 40.0 °C
Ejection Temperature 50.0 °C
Drying Temperature 70.0 - 110 °C
Dry Time 1.00 - 2.00 hourDry Air Dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 India
 Near East/Africa
 North America
 South and Central America
Eff. thermal diffusivity (m²/s)8E-08

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® W DP 89051D Polyurethane
Covestro Desmopan® 85786A Polyurethane
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Covestro Desmopan® 9873DU Polyurethane
Covestro Desmopan® 9385 Polyurethane

PB09826 / 92666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.