MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products MB 1150 Polyurethane Foam Modeling Board
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: MB 1150 is an Avocado colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1150 is low density foam of approximately 15lbs/ft3 board. Easily cut using CNC machining equipment or by hand the MB 1150 is perfectly suited for temporary master models, architectural design models, foundry patterns as well as design verification and prototype tools. Features: easily machined or hand carved, very little abrasion, no shrinkage, excellent at high speed cutting, excellent surface finish, exceptional dimensional stability. Uses: proofing intricate CNC designs, numerous tooling aids, temporary master models (automotive/aerospace), various prototypes, architectural models, foundry applications, bases for die models.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.240 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30
Tensile Strength, Ultimate 600 psi
Flexural Strength 780 psi
Compressive Strength 560 - 590 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°F
Maximum Service Temperature, Air 195 °F
Minimum Service Temperature, Air -300 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
BCC Products MB 1300 Polyurethane Foam Modeling Board
BCC Products MB 1100 Polyurethane Foam Modeling Board
Covestro Baynat® 3002 Polyurethane Foam

PBCC007 / 107234

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.