Hostacom DG 153 3 G62760 is an unfilled PP copolymer. Product is available as a customized color matched, pellet form. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in G62760 color version. Storage at high temperatures (> 50°C) and high humidity may damage the packaging.Information provided by LyondellBasell. |