MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Longitudinal Properties
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The corrosion resistance of carburized Pyrowear® 675 stainless is similar to that of Type 440C stainless, while the core toughness is similar to that of AISI 9310. In addition, the alloy provides excellent hot hardness capability. This alloy has been used in bearing and gear type applications.

Pyrowear® is a registered trademark of Carpenter Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.756 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 379Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 414Estimated from Rockwell C
Hardness, Rockwell C 41
Hardness, Vickers 396Estimated from Rockwell C
Tensile Strength, Ultimate 1276 MPa
Tensile Strength, Yield 1062 MPa
@Strain 0.2 %
Elongation at Break 20 %In 4D
Reduction of Area 75 %
Modulus of Elasticity 204 GPa
Fracture Toughness 138 MPa-m½K(Q)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.01 µm/m-°C
@Temperature 25.0 - 93.0 °C
 10.62 µm/m-°C
@Temperature 25.0 - 260 °C
 11.56 µm/m-°C
@Temperature 25.0 - 538 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.070 %
Chromium, Cr 13 %
Cobalt, Co 5.4 %
Iron, Fe 76 %as remainder
Manganese, Mn 0.65 %
Molybdenum, Mo 1.8 %
Nickel, Ni 2.6 %
Phosphorus, P <= 0.040 %
Vanadium, V 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
MetalTek MTEK 535 Martensitic Stainless Steel

NCARI2 / 15784

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.