Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties:- Good flow behavior
- Easy processing
- Short cycle times
Grilon BS 23 is suitable for thin wall applications, where excellent flow behavior and short cycle times are a must.Information provided by EMS Grivory. |