MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Silastic® LTC 9402-50 LSR Low_temperature-Cure Liquid Silicone Rubber  (discontinued **)
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: SILASTIC™ LTC 9400 Series LSRs are low-temperature-curing, high-strength elastomers that enable fast temperature activation in a wide temperature range.

Product applications:

  • Thick-walled connectors and seals
  • Electrical connector seals/gaskets
Key Features:
  • Low-temperature curing
  • Fast deep-section cure at standard elevated temperatures
  • Oil-filled: 2 wt %
  • Low compression set

Former Dow/ Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Viscosity 185000 cP
@Frequency 10 Hz
Part B; CTM 1094
 200000 cP
@Frequency 10 Hz
Part A; CTM 1094
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D2240
Tensile Strength 8.90 MPaASTM D412
Elongation at Break 450 %ASTM D412
Tear Strength 40.0 kN/mASTM D624 DIE B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® HV 1551-95P LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® LSR 9451-1000P Liquid Silicone Rubber
Dow Silastic® LCF 4630 Coating Liquid Silicone Rubber
Dow Silastic® HV 1523-30 LSR Electrical Grade Liquid Silicone Rubber
Dow Silastic® HV 1519-40 LSR Electrical Grade Liquid Silicone Rubber

PDOW9922 / 233125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.