MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake TRUCOAT® EC476 Extrusion Coating LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: TRUCOAT® EC476 is a low density polyethylene resin designed for extrusion coating and laminating applications where high coating speeds and good drawdown are required. It adheres well to paper, provides a good moisture barrier, and is heat-sealable at low temperatures.

Where required, test specimens are compression molded according to ASTM D 1928 at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Index of Compound 13.7 g/10 min13.7 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 8.96 MPa1300 psi500 mm/min (20 in/min); ASTM D638 Type IV Specimen
Elongation at Break 450 %450 %500 mm/min (20 in/min); ASTMD 638 Type IV Specimen
Flexural Modulus, 1% Secant 137.9 MPa20000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °FDSC Peak; ASTM D3418
Vicat Softening Point 84.0 °C183 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 329 °C<= 625 °FExtrusion coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8736 / 287846

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.