MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax Fiberfrax® 7001-M-5 High Purity Bulk Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax Bulk Fibers are manufactured to be used as feedstock in manufacturing processes or other applications where product consistency is critical. Manufactured on large, computer-controlled furnaces, these products provide customers with consistent material properties. Fiberfrax Bulk Fibers are typically used in the manufacture of other ceramic fiber based product forms such as:

  • High-temperature boards, felts, and papers
  • Combustion chambers for commercial and residential boilers
  • Riser sleeves for molten metal casting
  • Fireplace logs and panels for gas fireplaces
  • Tap out cones for molten metal applications
  • Specialized vaccum-formed shapes

These bulk fibers can also be directly used as high-temperature fill and packing material in a variety of high-temperature applications, such as:

  • Expansion joints
  • Furnace base seals
  • Tube seals
  • Burner tile packing
  • Chimney insulation

Fiberfrax 7000 Series fibers are manufactured from high-purity alumina-silica materials for use in applications up to 2300°F (1260°C). These products are manufactured on computer-controlled, state-of-the-art furnaces to provide customers with consistent fiber properties. Fiberfrax 7000 Series fibers can also be chopped into several grades (coarse, medium, and fine) to provide customers with a fiber ideally suited for their application. Benefits of Fiberfrax 7000 Series fibers include:

  • Low thermal shrinkage at high temperatures
  • Consistent fiber properties
  • Several chopped grades

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.73 g/cc2.73 g/cc
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1175 °C2147 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 47 - 52 %47 - 52 %
NaO2 <= 0.50 %<= 0.50 %
SiO2 48 - 53 %48 - 53 %
 
Descriptive Properties
Average Fiber Diameter (microns)1.5-2.5
ChoppingMedium
ColorWhite
Fiber Index (%)45-55
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CUNIF058 / 97830

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.