MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.

Features: Contains UV additives

Available in Americas

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 100 °C
10 g/10 min
@Load 4.76 lb,
Temperature 212 °F
ASTM D1230
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060Dry; ASTM D2240
Tensile Strength, Ultimate 5.17 MPa750 psiDry weak gel; ASTM D412
Elongation at Break 100 %100 %Dry weak gel; ASTM D412
 
Processing PropertiesMetricEnglishComments
Zone 1 100 °C212 °F
Zone 2 105 °C221 °F
Zone 3 110 °C230 °F
Zone 4 115 °C239 °F
Die Temperature 115 °C239 °F
Melt Temperature 115 °C239 °F
Drying Temperature 43.3 °C110 °Fforced air desiccant dryer
Dry Time 4.00 hour4.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane
BASF Elastollan® 890 AN TPUR

PNOVEON579 / 121470

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.