Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherability, excellent processabilityApplications: thermoformed sheet Description: Hifax ETA-4161UV fractional melt flow, UV-stabilized, extrusion grade thermoplastic olefin resin has an excellent combination of stiffness, impact resistane, melt strength, weatherability and processability. It was designed to accommodate specific thermoformed applications. Information provided by Montell Polyolefins. LyondellBasell is the successor company to Montell. |