MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Graft Polymer GRAFTABOND™ LD-MAH 00130 TL Highly functionalized polyethylene with maleic anhydride
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: GRAFTABOND™ LD-MAH 00130 TL is a coupling agent for polyethylene fiber/filler compound. Tie layer adhesive for multi-layer barrier films. Supplied as: Granulate. Applications: Compatibillizer in thermoplastic composites, compounds and alloys.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 0.50 - 3.0 g/10 minASTM D1238
 
Descriptive Properties
Drying Loss<0.5 g/cc. ASTM D6980.
Maleic Anhydride Graft Level2.5 to 3%, FTIR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ LD-MAH 02030 C Highly functionalized polyethylene with maleic anhydride
Graft Polymer GRAFTABOND™ HD-MAH 02030 C Highly functionalized polyethylene with maleic anhydride
Graft Polymer GRAFTABOND™ HD-GMA 02530 C Highly functionalized polyethylene with glycidyl methacrylate
Graft Polymer GRAFTABOND™ ECO 01030 C Polyolefin Based Universal Compatibilizer
Graft Polymer GRAFTABOND™ LL-MAH 00230 TL Linear Low Density Polyethylene (LLDPE) Grafted with Maleic Anhydride.

PGRAFT948 / 232379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.