System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ashley Polymers Ashlene® P284 PPE Alloy, 10% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Ether/PPO
;
Polyphenylene Ether, 10% Glass Filled
Material Notes:
A 10% glass reinforced PPE Alloy for superior properties and chemical resistance with high heat resistance.
Data provided by the manufacturer
Key Words:
Polyphenylene Oxide; Ashley Polymers, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.16
g/cc
0.0419
lb/in³
ASTM D792
Water Absorption
0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage
0.0075
cm/cm
0.0075
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
86.0
MPa
12500
psi
ATSM D638
Elongation at Break
9.0 %
9.0 %
ASTM D638
Flexural Strength
136
MPa
19700
psi
ASTM D790
Flexural Modulus
3.50
GPa
508
ksi
ASTM D790
Izod Impact, Notched
0.640
J/cm
1.20
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
250
°C
482
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
204
°C
399
°F
ASTM D648
Vicat Softening Point
239
°C
462
°F
ASTM D1525
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
RTP Company RTP 1700 TFE 10 FR Modified Polyphenylene Oxide (PPO), PTFE Lubricated - Flame Retardant
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass
PNAD23 / 54685
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.