MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NanoScale NanoActive® Cerium Oxide  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the particle size.

Applications: Applications include catalysts, enhancement of Near IR reflection, industrial coatings, polishing slurries, and reactive dopants.

Information provided by NanoScale

Composition based on metal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.20 g/cc0.0795 lb/in³
Density 6.00 g/cc0.217 lb/in³
Moisture Absorption <= 3.0 %<= 3.0 %
Loss On Ignition <= 5.0 %<= 5.0 %
Particle Size 9.5 µm9.5 µmmean aggregate size
Specific Surface Area >= 50 m²/g>= 50 m²/gBET
Pore Size 0.00700 microns0.000276 milAverage Diameter
 
Component Elements PropertiesMetricEnglishComments
Cerium, Ce >= 99.7 %>= 99.7 %
 
Descriptive Properties
Appearance / ColorYellow Powder
Crystallite Size= 7 nm
Minimum Total Pore Volume cc/g0.1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CNANO04 / 1666

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.