MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2256 Void Free High Temperature Thermally Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2256 is recommended for high temperature aerospace and electronic applications where the combination of easy application, high thermal conductivity and low electrical conductivity is required. This two part epoxy system bonds extremely well to ceramics, glass, metals and most plastics. The TRA-BOND 2256 develops durable, thermally conductive bonds with good impact properties. It is resistant to galvanic action, weathering, moisture, salt, mild alkalis and acids as well as many petroleum products.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 32500 cP
@Temperature 25.0 °C
Mixed (sp #14, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 951 hr @ 100°C + 1 hr @ 150°C
Adhesive Bond Strength 2000 psiLap shear, alum to alum, 1 hr @ 100°C + 1 hr @ 150°C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour1 hr @ 100°C + 1 hr @ 150°C
 
Descriptive Properties
Color Light Tan
Mix Ratio, parts by weight100/51Resin/Hardener
Outgassing, NASA Passes
Thixotropic Index 1.51 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC072 / 71000

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.