MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Purell RP370M Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Purell RP370M is a medium modified polypropylene random copolymer. It does not contain slip or anti-blocking additives. Purell RP370M is typically used by customers for manufacturing of un-oriented cast films and blown film extrusion. It has been reported by customers that Purell RP370M exhibits good processability, and that films produced with Purell RP370M exhibits high clarity and gloss, softness and good heat weldability.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Caps & Closures (Healthcare); Healthcare Applications; Infusion Bags; Medical Film

Market: Healthcare

Processing Method: Cast Film; Injection Molding

Attribute: Autoclavable; Ethylene Oxide Sterilization; Good Optical Properties; Medium Transparency

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 8.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPaISO 527-1, -2
Elongation at Break >= 50.0 %ISO 527-1, -2
Elongation at Yield 14.0 %ISO 527-1, -2
Tensile Modulus 850 MPaISO 527-1, -2
Charpy Impact, Notched 3.00 kJ/m²
@Temperature 0.000 °C
ISO 179-1/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 135 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9789 / 324724

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.