MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EMAC® SP2209 Specialty Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Compounding Grade

Material Notes: EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. For use as heat seal layer, adhesive layer, or modifier for cost/performance enhancement. They are soft, pliable and tough at ambient and freezing temperatures and exhibit excellent ESCR. These polymers exhibit high solids fillability and compatibility with a wide range of polymers. This facilitates their uses as bases for all-purpose concentrates for addition to a wide spectrum of polymers. They process like LDPE.

Applications/Uses

  • Films
  • Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.943 g/ccASTM D1505
    Methyl Acrylate Content 20 %
    Melt Flow 3.5 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 40ASTM D2240
    Tensile Strength at Break 11.0 MPaASTM D638
    Elongation at Break 777 %500mm/min; ASTM D638
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 83.0 °CDSC
    Vicat Softening Point 54.0 °C1kg load; ASTM D1525
    Brittleness Temperature <= -73.0 °CASTM D746

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
    Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
    Dow Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
    Dow Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
    Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating

    PE9070 / 35126

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.