Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resistance. Processing and stability with overall physical properties are excellent. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |