MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Acerde Aluminum Nitride
Categories: Ceramic; Nitride

Material Notes: Aluminum Nitride key properties: High thermal conductivity, Good resistance to abrasion and oxidation, Electrical insulating material, Low thermal expansion coefficient, Piezoelectric

Aluminum Nitride main applications domains: High temperature piezoelectric pressure sensors, Substrates for electronic packages, Opto-electronics: Deep UV LEDs, Heat sinks for the microelectronics, IC packages, Power transistor, Microwave device packages, Material processing kiln furniture, Semiconductor processing chamber fixtures and insulators, Molten metal handling components, Medical (echography)

Information provided by Acerde

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.26 g/cc
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1100[Kg/mm²]
Flexural Strength 320 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature <=1000 °C
Thermal Conductivity 285 W/m-K
Melting Point 3200 °CUnder High Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride
Aluminum Nitride, AlN
Sapco Aluminum Nitride
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride

CZACERD03 / 122021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.