MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® PR 435 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol PR 435 is an aqueous aliphatic polyurethane dispersion that contains only 5% by weight of organic cosolvent.

Properties / Applications: Bayhydrol PR 435 polyurethane dispersion has been developed especially for the formulation of water-borne air-dry or force-dry automotive refinish primer- surfaces. Automotive primer-surfaces based on Bayhydrol PR 435 display fast drying, good early sandability, abrasion resistance, durability and resistance to humidity. As with any product, use of Bayhydrol PR 435 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Volatiles 64 - 66 %
pH 7.0 - 9.0
Viscosity <= 400 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.7 MPa
Elongation at Break 200 %
100% Modulus 17.2 MPa
@Strain 100 %
 
Processing PropertiesOriginal ValueComments
Moisture Content 60 %
 
Descriptive Properties
Content5%n-methyl-2-pyrrolidone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0163 / 201946

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.