MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for applications where hard/oft combinations are required. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • Designed for excellent adhesion to PC, ABS, PC/ABS, ASA and PMMA (cold insert or 2K [two-shot] molding).
  • Broad processing window in injection molding.
  • Recommended for applications requiring superior part surface appearance.
  • UL listed, EU and China RoHS compliant.
Applications:
  • Automotive-Plugs, Bumpers, Grommets, Clips
  • Consumer-Floor Care, Kitchen Tools, Power Tools, Writing Instruments
  • Consumer Applications
  • Seals and Gaskets
  • Soft Touch Grips
Uses:
  • Appliance Components
  • Appliances
  • Automotive Applications
  • Automotive Under the Hood
  • Bonding
  • Cell Phones
  • Consumer Applications
  • Eyeglass Frames
  • Flexible Grips
  • Kitchenware
  • Living Hinges
  • Seals
  • Sporting Goods
  • Strain Reliefs
  • Tie-Layer
  • White Goods & Small Appliances
Processing Method: Coextrusion, Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792 and ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 15.0 sec
2 mm; ISO 868
Tensile Strength at Break 11.7 MPaAcross Flow; ASTM D412 and ISO 37
Tensile Stress at Strain 3.20 MPa
@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 570 %Across Flow; ASTM D412 and ISO 37
Tear Strength 46.0 kN/mAcross Flow, Die C; ASTM D624
 46.0 kN/mAcross Flow, Method Bb, Angle (Nicked); ISO 34-1
Compression Set 37 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B Type 1 and ISO 188 Type A
 68 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B Type 1 and ISO 188 Type A
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.60 mm
UL File Number - E80017
 HB
@Thickness 2.10 mm
 
Descriptive Properties
Change in Tensile Strength in Air-8.0%ASTM D573, 100°C, 168 hr
Change in Ultimate Elongation in Air-11%ASTM D573, 100°C, 168 hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate

PEXA918 / 125961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.