MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyChem Alloy PolyOxyter 2501
Categories: Polymer

Material Notes: PolyOxyter, an additive masterbatch product, has been specially formulated with reactive compounds to provide performance enhancement and processing improvement for Polyesters, Nylons, and Polycarbonates. The product has been formulated to provide performance enhancement in both extrusion and molding processes. When used at a typical 3% to 7% let-down, PolyOxyter has been shown to produce many impressive benefits, such as: a widened processing window, improved compatibility between dissimilar resins, controlled crystallinity and often crystallinity reduction, elimination of weld lines & warpage, frost line elimination and scrap reduction, stabilized melt viscosity, improved printability, improved dispersion of additives, increased loading capacity for fillers and additives, improved adhesion properties with polar surfaces, reduced hydrolytic breakdown, and enhanced clarity. PolyOxyter can also improve the properties of packaging materials. As an additive, the product can be co-extruded into multi-layered film with improved vapor barrier properties for enhanced resistance to moisture, oxygen, and carbon dioxide penetration, and improved interlayer film adhesion. When used with PET applications, PolyOxter controls crystallinity in the stretching process, reduces hydrolytic breakdown, improves surface adhesion, and optical compatibility. PolyOxyter is coextrudable with PET in cast and blown film operations, and can be applied by solution coating on PET for flexibility. PolyOxyter has a uniform pelletized shape, resembling a clear bead. The product has excellent compatibility with most any amorphous polymer system, such as polyester, polyamide, polycarbonate, polysulfone, polyethersulfone, polyketone, etc. PolyOxyter is manufactured using FDA compliant ingredients.

Key Words: PolyChem Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 1.20 g/cc>= 1.20 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 51.7 MPa7500 psi
Izod Impact, Notched 0.534 - 1.07 J/cm1.00 - 2.00 ft-lb/in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Saflex® Hurricane Interlayer
Overview of materials for Ionomer, Film Grade
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Honeywell ACCUGLASS® PTTY P-112A Spin-on Glass

PPC290 / 56076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.