MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Karina 822-18/599-CRB-LMP Gray PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Heavy metal free PVC compound.

Information provided by Karina Indústria e Comércio de Plásticos Ltda.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 - 1.39 g/ccASTM D 792
ASTM Color -2.16 - -0.160Color A, ME 12
 -1.99 - 0.010Color B, ME 12
 82.28 - 84.28Color L, ME 12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78 - 82
@Time 15.0 sec
ASTM D 2240
Tensile Strength >= 399 kg(f)/cm²ASTM D 638
Izod Impact, Notched >= 1.20 ft-lb/inMethod C, Resistance
 >= 54.0 ft-lb/inReversed Notch (Method E)
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 74.0 °CASTM D 1525
Heat Distortion Temperature >= 70.0 °CASTM D 648
Flammability, UL94 V-0
 
Descriptive Properties
ApplicationFittings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Karina 805-10/152-A-ERYB White PVC Compound
Overview of materials for Polypropylene, Extrusion Grade
Karina 837-10/119-E-ERYB White PVC Compound
Geon® Performance Solutions SF M7120 Polyvinyl Chloride, Rigid
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade

PKARIN9467 / 171123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.