MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 6 GF 35 TS Polyamide 6, 35% Glass Fiber, Thermal Stabilization  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Features

PA 6 for injection moulding, chemically reinforced with 35% glass fiber, heat stabilized, mouldings resistant against long-time heat impact up to 170°C. Used in environment, where long-time temperatures up to 150°C occur. Decrease in tensile strength by 50% after 5000 hours at 170°C. Application: grips of electrotools, hobby tools, gears, covers of electric appliances. Heat stabilization predetermines these products to an environment with long time heat stress like intake piping, cylinder heads, induction coils, carrying parts in the motor, fixing in the motor area. Delivered in black color.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0061 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0145 cm/cmSTN 64 0808
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 175 MPaSTN EN ISO 527-2
Elongation at Break 2.0 %STN EN ISO 527-2
Tensile Modulus 8500 MPaSTN EN ISO 527-2
Flexural Strength 200 MPaSTN EN ISO 178
Flexural Modulus 6500 MPaSTN EN ISO 178
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 65.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 11.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+13 ohm-cmSTN IEC 60093
Surface Resistance 8.00e+13 ohmSTN IEC 60093
Dielectric Strength 20.0 kV/mmSTN IEC 60243
Comparative Tracking Index 575 VSTN 34 6468
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °CSTN EN ISO 75/A
Vicat Softening Point 210 °CB; STN EN ISO 306
Flammability, UL94 HB
Glow Wire Test 650 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant
Albis Plastics Polyamide 6 PA 45/1 GF 35 , 35% Glass Fiber, Conditioned
Albis Plastics Polyamide 6 PA 45/1 GF 35 , 35% Glass Fiber, DAM
Avient Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6)
Avient Nymax™ GF 604 35 HS Black 13 Polyamide 6 (Nylon 6)

PPLACO020 / 106898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.