MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips Sumika Marlex® BPC-45 Polypropylene Talc-Filled Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polypropylene Talc-Filled Impact Copolymer

Applications: Formulated for Automotive Interior Door Panel Applications

The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Data provided by Phillips Sumika Polypropylene Company (PSPC).

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
@Thickness 3.20 mm
3.2 mm thick injection-molded specimen; ISO 1183
Linear Mold Shrinkage 0.0011 cm/cm100 x 100 mm Plaque, After 72 hrs.; 4.0 mm thick injection-molded specimen; ISO 257
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92
@Thickness 3.20 mm
3.2 mm thick injection-molded specimen; ISO 2039
Tensile Strength, Yield 21.0 MPa
@Thickness 4.00 mm
Type A Specimen, Rate: 5 mm/min; 4.0 mm thick injection-molded specimen;; ISO 527
Elongation at Break 21 %
@Thickness 4.00 mm
Type A Specimen, Rate: 5 mm/min; 4.0 mm thick injection-molded specimen;; ISO 527
Flexural Modulus 2.07 GPa
@Thickness 4.00 mm
Tangent; Rate 2.0 mm/min; injection-molded specimen; ISO 178
Izod Impact, Notched (ISO) 2.10 kJ/m²
@Thickness 4.00 mm,
Temperature -40.0 °C
injection-molded specimen; ISO 180
 2.10 kJ/m²
@Thickness 4.00 mm,
Temperature 0.000 °C
4.0 mm thick injection-molded specimen; ISO 180
Izod Impact Resistance 0.550 J/cm²
@Thickness 4.00 mm
injection-molded specimen; ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
@Thickness 4.00 mm
4.0 mm thick injection-molded specimen; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
@Thickness 4.00 mm
4.0 mm thick injection-molded specimen; ISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled

PCHEVS28 / 20366

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.