MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Lemalloy® BX528A-3 PPE-PA6 Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Polyphenylene Ether/PPO

Material Notes: PPE-PA6 Alloy, standards. Lemalloy provides well-balanced mechanical, electrical, and thermal properties. In addition, Lemalloy boasts the lowest specific gravity among engineering plastics. Equipped with the above features, Lemalloy meets market requirements for compactness, high performance, and flame retardance. Stable rigidity, impact strength and fatigue resistance through a wide range of temperatures. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Excellent heat stability. Low specific gravity. Excellent moldability and low shrinkage rate for quality precision parts. Excellent processability; good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.115 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
@Thickness 3.20 mm
Melt Flow 28 g/10 min
@Load 5.00 kg,
Temperature 280 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 37.0 MPa50% RH; ISO-527-1,2
 62.0 MPadry; ISO-527-1,2
Elongation at Break 57 %dry; ISO 527-1,2
 140 %50% RH; ISO 527-1,2
Elongation at Yield 5.0 %dry; ISO 527-1,2
 14.9 %50% RH; ISO 527-1,2
Tensile Modulus 1400 MPa50% RH; ISO 527-1,2
 2500 MPadry; ISO 527-1,2
Flexural Strength 60.0 MPa50% RH; ISO 178
 91.0 MPadry; ISO 178
Flexural Modulus 1400 MPa50% RH; ISO 178
 2300 MPadry; ISO 178
Charpy Impact, Notched 18.0 kJ/m²dry; ISO 179-1,2
 66.0 kJ/m²50% RH; ISO 179-1,2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 165 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Fiberfil® M-2450 Polypropylene Copolymer
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Mitsubishi Lemalloy® C61HL PPE-PA66 Alloy
Envalior Durethan® CI 31 F 000000 Copolyamide PA6/6I
Envalior Durethan® BC 40 SR2 000000 Nylon 6 (PA6), Dry

PMITSU9166 / 191839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.