MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® TBR-605CS with 10 phr N990 Carbon Black and 20 phr Austin Carbon Black  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® Extreme™ TBR-605CS (formerly VTR-8802) is a base-resistant TFE/propylene polymer, containing a proprietary bisphenol curative. Viton® Extreme™ TBR-605CS utilizes a bisphenol cure site, together with optimized molecular architecture, to provide a polymer that:
  • Cures quickly, to a high state of cure
  • Exhibits excellent mold release and low mold fouling
  • Is inherently resistant to attack by basic chemicals
  • Provides excellent heat resistance
  • Provides superior resistance to hydrocarbon oils compared to other TFE-propylene polymers
  • Provides excellent compression set resistance

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015. This specific grade had been discontinued prior to the spinoff.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Tensile Strength, Ultimate 13.4 MPa1940 psiCured 10 min at 177°C and Post Cured 24 hr at 232°C
Elongation at Break 180 %180 %Cured 10 min at 177°C and Post Cured 24 hr at 232°C
50% Modulus 4.50 MPa
@Strain 50 %
4.50 MPa
@Strain 50 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
100% Modulus 9.20 MPa
@Strain 100 %
1330 psi
@Strain 100 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 22 %
@Temperature 200 °C
22 %
@Temperature 392 °F
Method B, O-rings, 70 hr
 
Descriptive Properties
Formulation as Tested10MT (N990) Carbon Black
 100Viton® Extreme™ TBR-605CS
 20Austin Carbon Black
 8High-Activity MgO

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDVDA41 / 34010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.