MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kazanorgsintez 153-02 K Polyethylene Composition for Cable Industry
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives.

Application: Compositions are used for lapping, cable sheaths, and serving by extrusion method.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9185 - 0.922 g/ccPremium Quality
 0.9185 - 0.992 g/ccSuperior Quality
Environmental Stress Crack Resistance >= 500 hour
Melt Flow 0.21 - 0.39 g/10 min±8% Superior Quality, ±12% Premium Quality
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 11.3 MPa
Elongation at Break >= 600 %
Tear Strength Test >= 14.7MPa
 
Descriptive Properties
Amount of impurities [pcs]15Premium Quality
 3Superior Quality
Extractable Substance Weight Content (%)1.4Superior Quality
 1.7Premium Quality

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAZAN039 / 127358

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.