MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Microcell Composite Company CELLAMP® M5110 Thermoplastic Foam
Categories: Polymer; Thermoplastic

Material Notes: CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high damping characteristics. It is comfortable to the touch and has contour form memory characteristics.

Information provided by Microcell Composite Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.100 - 0.140 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore C 17 - 21ASTM D2240
Tensile Strength, Yield 4.00 kg(f)/cm²ASTM D412
Elongation at Yield 200 %ASTM D412
Tear Strength 2.00 kg(f)/cmASTM D624
Compression Set 90 %
@Temperature 70.0 °C,
Time 21600 sec
50%; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.0 %
@Temperature 70.0 °C,
Time 2400 sec
ASTM D1204
 
Descriptive Properties
Resiliency (%)25ASTM D2632

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Microcell Composite Company CELLIFF® F7010 Polymer Foam
Microcell Composite Company CELLIFF® F-1020ST Polymer Foam
Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam
Armacell OleTex® BKJN 200 LDPE Foam

PMCELL12 / 108449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.