MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Glass Filled

Material Notes: Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature Impact

Uses: Injection Molding

Availability: Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Filler Content 30 %Glass Fiber
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.00040 cm/cmflex bar; ASTM D955
 0.0010 cm/cmaverage flow and against flow, disc; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72 - 78
@Time 5.00 sec
ASTM D2240
Tensile Strength 83.0 MPaASTM D638
Elongation at Break 20 %ASTM D638
Tensile Modulus 530000 psiASTM D638
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 420000 psiASTM D790
Izod Impact, Notched 8.00 ft-lb/inASTM D256
 2.40 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 °C
Middle Barrel Temperature 221 °C
Front Barrel Temperature 224 °C
Nozzle Temperature 232 °C
Melt Temperature 232 °C
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy

PNOVEON004 / 55269

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.