GRAFTALEN™ MP-UHHD is a high performance polymer alloy, consisting of ultra-high molecular weight polyethylene and high density polyethylene. Its main characteristics are very high impact strength, which remains high even at low temperatures, and great flexural properties. Applications: GRAFTALEN™ MP-UHHD functions as a toughener Improves mechanical characteristicsIncreases abrasion resistance. Supplied as Granulate.Information provided by Graft Polymer LTD. |