MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/ccISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0020 cm/cmEurotec
Linear Mold Shrinkage, Transverse 0.0090 cm/cmEurotec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527
Elongation at Break 1.5 %ISO 527
Tensile Modulus 13000 MPaISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1U
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Comparative Tracking Index 200 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °C[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75
Flammability, UL94 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.60 mm
Glow Wire Ignition Temperature 775 °C
@Thickness 2.00 mm
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 280 °C
Feed Temperature 50.0 - 70.0 °CThroat
Mold Temperature 120 - 140 °C
Drying Temperature 120 - 140 °C
Dry Time 4.00 hour
Moisture Content <= 0.080 %ISO 960
Hold Pressure 60.0 - 100 MPa
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced
Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0
Celanese FORTRON 1342L4 PPS, 40% Specialty
Avient OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS)

PEUROS142 / 147132

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.