MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV 4190 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4100 series are engineered materials designed primarily for demanding automotive and industrial applications. Available in both black and natural, this product is a low density, higher hardness thermoplastic vulcanizate featuring excellent flex fatigue resistance, heat aging, improved elasticity and resilience. It can be used in injection molded parts, sheet and profile extrusion such as weather-stripping and expansion joints, and can also be blow molded into boots and ducts.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Excellent Elastic Recovery; Fatigue Resistant; Good Adhesion; Good Flexibility; Good Melt Strength; Good Moldability; Good Processability; Good Surface Finish; Heat Aging Resistant; High Hardness; High Melt Stability; Low Density; Low Specific Gravity; Low Temperature Flexibility; Medium Heat Resistant; Resilient

Uses: Agricultural Applications; Appliance Components; Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Gaskets; Industrial Applications; Pipe Seals; Profiles; Rubber Replacement; Sheet; Weatherstripping; White Goods & Small Appliance

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 EGN Color: Black; CHRYSLER MS-AR-100 EGN Color: Natural; FORD WSD-M2D382-A1 Color: Black; FORD WSD-M2D382-A1 Color: Natural; GM GMP.E/P.005 Color: Black; GM GMP.E/P.005 Color: Natural; GM GMW/15813 Type 8 Color: Black; GM GMW/15813 Type 8 Color: Natural; GM QK 3526 Type 6 Color: Black; GM QK 3526 Type 6 Color: Natural

UL File Number: QMFZ2. E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding; Blow Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Viscosity 340 cP
@Shear Rate 206 1/s,
Temperature 200 °C
340 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  86
@Time 5.00 sec
86
@Time 0.00139 hour
Extruded; ASTM D2240
 90
@Time 5.00 sec
90
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 13.6 MPa1970 psiFlow; ASTM D412
 14.5 MPa2100 psiAcross Flow; ASTM D412
 12.9 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
1870 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
 13.3 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
1930 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  6.70 MPa
@Strain 100 %
972 psi
@Strain 100 %
Across Flow; ISO 37
 10.2 MPa
@Strain 100 %
1480 psi
@Strain 100 %
Flow; ISO 37
 7.37 MPa
@Strain 100 %,
Treatment Temp. 150 °C
1070 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 7.71 MPa
@Strain 100 %,
Treatment Temp. 135 °C
1120 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 380 %380 %Flow; ASTM D412
 650 %650 %Across Flow; ASTM D412
 540 %
@Treatment Temp. 150 °C,
Time 605000 sec
540 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 546 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
546 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Poissons Ratio 0.430.43ASTM E132
Tear Strength 71.9 kN/m410 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  36 %
@Temperature 22.8 °C,
Time 79200 sec
36 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 48 %
@Temperature 70.0 °C,
Time 79200 sec
48 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 72 %
@Temperature 125 °C,
Time 252000 sec
72 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.39
@Thickness 2.00 mm
2.39
@Thickness 0.0787 in
ASTM D150
Dielectric Strength 20.5 kV/mm
@Thickness 2.00 mm
520 kV/in
@Thickness 0.0787 in
ASTM D419
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.02 mm
HB
@Thickness 0.0400 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 227 °C360 - 440 °FInjection
Rear Barrel Temperature 138 - 160 °C280 - 320 °FInjection
Middle Barrel Temperature 166 - 193 °C330 - 380 °FInjection
Front Barrel Temperature 177 - 227 °C350 - 440 °FInjection
Nozzle Temperature 182 - 227 °C360 - 440 °FInjection
Zone 1 180 - 200 °C356 - 392 °FExtrusion
Zone 2 180 - 205 °C356 - 401 °FExtrusion
Zone 3 187 - 210 °C369 - 410 °FExtrusion
Zone 4 187 - 210 °C369 - 410 °FExtrusion
Die Temperature 195 - 215 °C383 - 419 °FExtrusion
Melt Temperature 195 - 215 °C383 - 419 °FExtrusion
Mold Temperature 15.6 - 54.4 °C60.0 - 130 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 25 - 75 rpm25 - 75 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer

PTEKNQ1161 / 237652

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.