MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsui Polypropylene Modified w/ NOTIO™  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polyolefin elastomer. NOTIO™ is a controlled crystal and amorphous structure on a nano scale, and shows better properties when compared with conventional polyolefin elastomers. The property values below are for the Notio-PP 80/20(wt%) blend.

Information provided by Mitsui Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57
Tensile Strength at Break 30.0 MPa
Tensile Strength, Yield 18.0 MPa
Elongation at Break >= 550 %
Elongation at Yield 11 %
Modulus of Elasticity 0.580 GPa
Izod Impact, Notched 65.0 J/m
Abrasion 94Scratch resistance, % Load=1kgf reciprocating times=10; JIS L 0849 Frictional wear test
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 138 °CTMA needle insertion temperature
Vicat Softening Point 114 °C
 
Optical PropertiesOriginal ValueComments
Haze 74 %
@Thickness 2.00 mm
Press molding sheet

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui ADMER® QF551A PP Type Polyolefin
Sibur APP-B Atactic Polypropylene
Multibase Multi-Flam™ 205 HFRI Polypropylene
Mitsui ADMER® QF500A PP Type Polyolefin
Mitsui ADMER® QB520A PP Type Polyolefin

PMIT151 / 53303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.