MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lubriplate 1444 Aluminum Complex Multi-Purpose Grease
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: Tacky aluminum complex grease specifically formulated for heavy-duty construction and mining equipment. Excellent for slow to moderate speed bearings and chains that are subjected to heat, steam, and water.

Applications: Heavy-duty construction, mining equip.

1444 is available in Cartridges, Pails, 1/4 Drums & Drums.

Information provided by Lubriplate

Key Words: Part Number L0227-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 3300 SUS
Kinematic Viscosity at 40°C (104°F) 626 cSt
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 265Unknown Amount of Work
Penetration P(60), 1/10 mm 295Unknown Amount of Work
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air 10.0 °FApprox. Cold test
Dropping Point 500 °FASTM Test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW/EP
NLGI Grade2
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Prodways PLASTCure Alumina Powder for 3D Printing
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
EOS PH1 Precipitation Hardening Stainless Steel Sintered on EOSINT M 270
Avient Versaflex™ CL30 Thermoplastic Elastomer (TPE)

WLUBR052 / 76098

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.