MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pressure Seal 9765 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9765 is a 70 durometer cream colored Fluoroelastomer, it is formulated with FDA approved materials. It exhibits good resistance to petroleum based oils and aromatic fuels. This compound is also suitable for milk and edible oils.

This compound will meet or exceed the specifications listed and has the following physical properties: 3-A Sanitary 18-03 Class I, II, III, & IV
CFR 21 177.2600

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.16 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
 68
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 68
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
 70
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
 70
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 71
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 75
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 75
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
Tensile Strength 1371 psi
 1110.5 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 1190 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 1222.9 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 1335.4 psi
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
 1365.5 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 1450.5 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 1684.9 psi
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 259 %
 186 %
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
 202 %
@Treatment Temp. 200 °C,
Time 252000 sec
Stauffer Blend 7700
 220.9 %
@Treatment Temp. 200 °C,
Time 252000 sec
Service Fluid 101
 231.1 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 232.1 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 247.1 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 367 %
@Treatment Temp. 275 °C,
Time 252000 sec
Heat Aged
100% Modulus 608 psi
Tear Strength 151 pliDie C
 204 pliDie B
Compression Set 13.5 %
@Treatment Temp. 23.0 °C,
Time 79200 sec
Plied
 61 %
@Treatment Temp. 175 °C,
Time 79200 sec
Plied
 76.5 %
@Treatment Temp. 200 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature 7.00 °F
Shrinkage 0.00 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 1.4 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 1.8 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 3.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 9.4 %
@Treatment Temp. 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 17 %
@Treatment Temp. 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL125 / 318335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.